订货号 Order No. | D | d | L | L1 | 订货号 Order No. | D | d | L | L1 |
JWS/3.00 | 3.00 | 4 | 60 | 30 | JWS/3.75 | 3.75 | 4.5 | 65 | 32 |
JWS/3.05 | 3.05 | 4 | 60 | 32 | JWS/3.80 | 3.80 | 4.5 | 65 | 40 |
JWS/3.10 | 3.10 | 4 | 60 | 32 | JWS/3.85 | 3.85 | 4.5 | 65 | 40 |
JWS/3.15 | 3.15 | 4 | 60 | 32 | JWS/3.90 | 3.90 | 4.5 | 65 | 40 |
JWS/3.20 | 3.20 | 4 | 60 | 32 | JWS/3.95 | 3.95 | 4.5 | 65 | 40 |
JWS/3.25 | 3.25 | 4 | 60 | 32 | JWS/4.00 | 4.00 | 5 | 70 | 40 |
JWS/3.30 | 3.30 | 4 | 60 | 32 | JWS/4.05 | 4.05 | 5 | 70 | 40 |
JWS/3.35 | 3.35 | 4 | 60 | 32 | JWS/4.10 | 4.10 | 5 | 70 | 40 |
JWS/3.40 | 3.40 | 4 | 60 | 32 | JWS/4.15 | 4.15 | 5 | 70 | 40 |
JWS/3.45 | 3.45 | 4 | 60 | 32 | JWS/4.20 | 4.20 | 5 | 70 | 40 |
JWS/3.50 | 3.50 | 4.5 | 65 | 32 | JWS/4.25 | 4.25 | 5 | 70 | 40 |
JWS/3.55 | 3.55 | 4.5 | 65 | 32 | JWS/4.30 | 4.30 | 5 | 70 | 40 |
JWS/3.60 | 3.60 | 4.5 | 65 | 32 | JWS/4.35 | 4.35 | 5 | 70 | 40 |
JWS/3.65 | 3.65 | 4.5 | 65 | 32 | JWS/4.40 | 4.40 | 5 | 70 | 40 |
JWS/3.70 | 3.70 | 4.5 | 65 | 32 | JWS/4.45 | 4.45 | 5 | 70 | 40 |
金刚石刀具小编对于一般切削深度不该越过磨料自身颗粒尺度的1/3~1/4,否则会因积屑过多而把高速钢五方铰刀卡在工件孔中,使刀具寿数下降,通常用80#~120#粒度的高速钢五方铰刀,其加工余量可达0.02~0.04mm,对170#~270#粒度的高速钢五方铰刀,加工余量为0.015~0.025mm,对325#~400#粒度的高速钢五方铰刀,其加工余量不该越过0.005~0.01mm。
1.高速钢五方铰刀在孔中往复次数不该过多
一般状况下一次往复行程即可,现在不少操作者把这种高速钢五方铰刀作研磨棒来运用,由于过多添加往复次数,会使高速钢五方铰刀的寿数下降。
2.挑选合理的切削液
铰削铸铁孔时,可用80%火油和20%硫化油或机械油的混台油作切削液,或悉数火油也可,加工钢件时,可用70%火油加30%硫化油,应该指出,因立方氮化硼易和水蒸气板响而生成氨和硼酸,所以不该用水作切削液,切削液应供给足够,并要过滤,以确保刀具的运用寿数和工件加工的质量。